Research Article

The Effect of Exposed Glass Fibers and Particles of Bioactive Glass on the Surface Wettability of Composite Implants

Table 3

Mean values and standard deviations (SD) of the specimens’ surface roughness recorded with a confocal image profiler.

GroupsMean roughness, μm (SD)
Photo polymerizedPostpolymerized by heat

(1) Polymer with in-plane oriented fibers0.061 (0.013)0.037 (0.008)
(2) Polymer with transversely oriented fibers0.024 (0.003)0.018 (0.004)
(3) 100% polymer (BisGMA-TEGDMA)0.006 (0.001)0.008 (0.001)
(4) 75% polymer + 25 wt. % fraction of BAG-particles0.035 (0.008)0.051 (0.021)
(5) 50% polymer + 50 wt. % fraction of BAG-particles0.042 (0.003)0.096 (0.026)
(6) 25% polymer + 75 wt. % fraction of BAG-particles0.088 (0.012)0.045 (0.018)

(7) 100% BAG*0.012 (0.003)

*No curing.