Research Article

In Vitro Evaluation of Some Types of Ferrimagnetic Glass Ceramics

Figure 2

(a) SEM micrograph of Ca-doped glass ceramics (A) before, (B) after 1 week, (C) after 2 weeks, and (D) after 4 weeks of immersion in SBF. (b) EDAX of Ca-doped glass ceramics after 4-week immersion in SBF.
415854.fig.002a
(a)
415854.fig.002b
(b)