415854.fig.006a
(a)
415854.fig.006b
(b)
Figure 6: (a) SEM micrograph of Ce-doped glass ceramics (A) before, (B) after 1 week, (C) after 2 weeks, and (D) after 4 weeks of immersion in SBF. (b) EDAX of Ce-doped glass ceramics after 4-week immersion in SBF.