Cuspal Displacement Induced by Bulk Fill Resin Composite Polymerization: Biomechanical Evaluation Using Fiber Bragg Grating Sensors

Table 1

Materials composition.

Resin compositeManufacturerResin matrixFillerBatch #

SDR
Microhybrid
Dentsply
DeTrey
Modified
UDMA
EBPADMA
TEGDMA
Ba-Al-F-B-Si-glass
Sr-Al-F-Si-glass
(68 wt%., 45 vol%)
1105141
Esthet•X® HD 
Microhybrid
Dentsply
DeTrey
Bis-GMA adduct
Bis-EMA adduct
TEGDMA
Ba-F-Al-B-Si-glass
Nanofiller silica
(77 wt%; 60 vol%)
1006292

AdhesiveManufacturerChemical compositionInstructionsBatch #

Prime&Bond®NT
2-step etch and rinse adhesive
Dentsply
DeTrey
Di- and trimethacrylate resins
PENTA
Photoinitiators
Stabilizers
Nanofillers
Acetone
Apply 36% phosphoric acid for 15 seconds; spray and rinse with water for 15 seconds; blot dry conditioned areas; apply adhesive and leave the surface wet for 20 seconds; gently dry for at least 5 seconds; polymerize for 10 seconds; apply a second layer of adhesive1109001528

Bis-GMA (bisphenol A dimethacrylate); Bis-EMA (bisphenol A polyethylene glycol diether dimethacrylate); UDMA (urethane dimethacrylate); TEGDMA (triethylene glycol dimethacrylate); EBPADMA (ethoxylated bisphenol A dimethacrylate).