Research Article

Shear Bond Strengths between Three Different Yttria-Stabilized Zirconia Dental Materials and Veneering Ceramic and Their Susceptibility to Autoclave Induced Low-Temperature Degradation

Table 8

Comparison of surface grain size (µm) of zirconia in all the groups showing mean, standard deviation, and significance for the samples within subgroups.

Upcera Ziecon Cercon value (significance < 0.05)

Comparison in between subgroups without artificial aging
Mean (µm) ± SD0.43 ± 0.039 0.41 ± 0.064 0.39 ± 0.060 0.532

Comparison in between subgroups with artificial aging
Mean (µm) ± SD0.42 ± 0.0340.40 ± 0.05 0.40 ± 0.032 0.781