Examples of previously reported conditions for GA vapour stabilisation of collagen and gelatine materials.
| Substrate | Format | Temperature | % GA | Time | Reference |
| Collagen (Limed bovine) | Reconstituted Fibrils | RT | 25% | 24 h, 48 h | Kato et al. [19] | Collagen (Bovine) | Reconstituted Fibrils | RT | 25% | 96 h | Law et al. [33] | Collagen (Bovine) | Film | 37°C | 8% | Various 3 h to 72 h | Barbani et al. [20] | Collagen (Bovine) | Electrospun mat | RT | (Not stated) | 24 h | Matthews et al. [34] | Collagen (Bovine) | Sponges | RT | 25% | 4 h, 8 h, 24 h | Lickorish et al. [21] | Collagen (Bovine) | Reconstituted Fibrils | RT | 25% | Various, 1 h to 24 h | Rho et al. [35] | Collagen (Bovine) | Electrospun mat | RT | 25% | 24 h | Yang et al. [36] | Bacterial Collagen | Sponge | RT | 20% | 18 h | Peng et al. [7] | Collagen (Bovine) | Electrospun mat | RT | 25% | 8 h | Takeda et al. [37] | Gelatine (Fish skin) | Electrospun mat | 37°C | 50 vol% | 3 h | Songchotikunpan et al. [22] | Gelatine | Electrospun mat | | 0.5% | 19 h | Sisson et al. [38] | Gelatine (Porcine) | Electrospun mat | 37°C | “Saturated” | 5 min | Dheraprasart et al. [39] | Gelatine (A-type, B-type) | DHT-treated Electrospun mat | 4°C | 0.06% in acetone/HCl | 48 h | Ratanavaraporn et al. [40] | Gelatine (A-type) | Electrospun mat | RT | 1.5% in EtOH | 48 h | Zha et al. [23] | Gelatine (Fish skin) | Electrospun mat | 40°C | 5% | Various, 0.5 h to 24 h | Gomes et al. [24] | Gelatine (Fish skin) | Electrospun mat | 40°C | 5% | 5 h | Gomes et al. [41] |
|
|
RT: Room temperature.
|