Research Article

Hot Corrosion Behavior of High-Chromium, High-Carbon Cast Irons in NaCl-KCl Molten Salts

Figure 5

X-ray patterns of corrosion products formed on cast irons containing 4.27, 4.06, 3.97 CE and on 304-type stainless steel exposed to NaCl-KCl at 670°C during 96 h.
479761.fig.005