Research Article

Hot Corrosion Behavior of High-Chromium, High-Carbon Cast Irons in NaCl-KCl Molten Salts

Figure 6

Micrograph of cast iron containing 3.97 CE-corroded NaCl-KCl at 670°C during 96 h together with X-ray mappings of Fe, Cr, O, and Cl.
479761.fig.006a
(a)
479761.fig.006b
(b)
479761.fig.006c
(c)
479761.fig.006d
(d)
479761.fig.006e
(e)