Research Article

Hot Corrosion Behavior of High-Chromium, High-Carbon Cast Irons in NaCl-KCl Molten Salts

Figure 8

Micrograph of cast iron containing 5.21 CE-corroded NaCl-KCl at 670°C during 96 h together with X-ray mappings of Fe, Cr, O, and Cl.
479761.fig.008a
(a)
479761.fig.008b
(b)
479761.fig.008c
(c)
479761.fig.008d
(d)
479761.fig.008e
(e)