Research Article

Effect of Microstructure on the Localized Corrosion and Stress Corrosion Behaviours of Plasma-Electrolytic-Oxidation-Treated AA7075 Aluminum Alloy Forging in 3.5 wt. % NaCl Solution

Figure 7

Stereo photomicrographs showing (a) localized pitting on the uncoated alloy, (b) crack initiation from localized corrosion, and (c) absence of pitting on the PEO-coated AA7075 aluminum alloy surface after SSRT (mag. 20x for (a) and (c).
823967.fig.007a
(a)
823967.fig.007b
(b)
823967.fig.007c