Research Article

The Corrosion Performance of Galvanized Steel in Closed Rusty Seawater

Figure 10

SEM and EDS analysis of galvanized steel immersed in CRS solution in 0.1 MPa. (a) SEM image of galvanized steel before immersion; (b) EDS result of (a); (c) SEM image of galvanized steel immersed in CRS solution at 0.1 MPa hydrostatic pressures after 14 days; (d) EDS result of (c) in the pitting area.
267353.fig.0010a
(a)
267353.fig.0010b
(b)
267353.fig.0010c
(c)
267353.fig.0010d
(d)