Research Article

Electrochemical and Oxidation Behavior of Yttria Stabilized Zirconia Coating on Zircaloy-4 Synthesized via Sol-Gel Process

Figure 2

XRD spectra of YSZ powders sintered at (a) 150°C, (b) 400°C, and (c) 700°C. The amorphous to crystalline transformation from 150°C to 400°C is clearly shown. The intensity of peaks increases from 400°C to 700°C.
453835.fig.002