EIS parameters for Ti6Al4V alloy in normal saline solution in the absence and presence of 25% and 50% Listerine at 1 h and 24 h of immersion.

System (Ω cm) (Ω cm2)   

Normal saline (1 h)19.20 0.919
Normal saline + 25% Lis. (1 h)19.24 0.883
Normal saline + 50% Lis. (1 h)41.25 0.854
Normal saline (24 h)10.10 0.925
Normal saline + 25% Lis. (24 h)23.70 0.906
Normal saline + 50% Lis. (24 h)37.51 0.862