Concrete properties and mix design.

Strength 25 N/mm2
Aggregate type: coarseCrashed
Aggregate type: fineCrashed
Free water-cement ratio 0.59
Slump: 30–60 mm, VB (time)3–6 second
Max aggregate size20 mm
Free water content 210 kg/m3
Cement content (C1) 355 kg/m3
Concrete density 2400 kg/m3
Total aggregate content 1834.09 kg/m3
Fine aggregate content 3514.7 kg/m3
Coarse aggregate content 1052.10 kg/m3
Curing time 28 days