Research Article

Sealing of PEO Coated AZ91 Magnesium Alloy Using La-Based Solutions

Figure 12

XPS survey scan for the PEO treated sample and for the sample sealed in an aqueous solution with 12 g/l of La(NO3)3 at 50°C for 30 minutes.