| Group - (mm) | Specimen ID No. | Concrete cover (mm) | Dimension (mm) |
| Confined | | 50 | | I – 16mm | A-1 | A-2 | A-3 | II – 20mm | B-1 | B-2 | B-3 | III –25mm | C-1 | C-2 | C-3 | Unconfined | | IV-16mm | D-1 | D-2 | D-3 | V – 20mm | E-1 | E-2 | E-3 | VI -25mm | F-1 | F-2 | F-3 |
|
|