Research Article
Combination of Natural and Thermosensitive Polymers in Flocculation of Fine Silica Dispersions
Figure 5
Transmission profiles of Aerosil OX50 at 300 rpm and T 25°C: (a) Aerosil OX50 + 0.2 mg/g CH2500 and (b) Aerosil OX50 + 0.2 mg/g CH2500 + 0.8 mg/g PNVCL.