Sample description.

Sample nameUnderlying surfaceSurface modification

TSTurned titaniumNone
TS + 8 nmTurned titaniumSpin coated with 8 nm TiO2 particles
TS + 22 nmTurned titaniumSpin coated with 22 nm TiO2 particles
TS + P25Turned titaniumSpin coated with P25 particles
TS + AT-ITurned titaniumTreated sequentially in oxalic and hydrofluoric acid [16]
AuMechanically polished goldNone
Au + 22 nmMechanically polished goldSpin coated with 22 nm TiO2 particles