(a) XPS survey scan and Sn3d5/2 spectra (inset) of (i) as-grown ITO film, (ii) after 30 minutes diamond growth on ITO substrate, (iii) after 1 hour hydrogen plasma treatment at 800°C, (iv) after two hours diamond growth on ITO substrate. (b) XPS survey scan and O1s spectra (inset) of (i) as-prepared AZO film, (ii) after 5 minutes and (iii) 10 minutes hydrogen plasma treatment at 800°C in an HFCVD reactor, (iv) after 30 minutes diamond growth on AZO substrate.