Research Article

High Tap Density Spherical Cathode Material Synthesized via Continuous Hydroxide Coprecipitation Method for Advanced Lithium-Ion Batteries

Figure 4

SEM of [Ni0.5Mn0.3Co0.2](OH)2 precursor at different magnifications (a) 500X, (b) 5000X, and (c) 10,000X.
323560.fig.004a
(a)
323560.fig.004b
(b)
323560.fig.004c
(c)