High Tap Density Spherical Cathode Material Synthesized via Continuous Hydroxide Coprecipitation Method for Advanced Lithium-Ion Batteries

Figure 8

Initial charge and discharge profiles of Li/Li[Ni0.5Mn0.3Co0.2]O2 cell at a current density of 0.2 C rate under different limiting conditions: (a) 3.0–4.3 V at 25°C, (b) 2.5–4.6 V at 25°C, and (c) 3.0–4.3 V at 55°C.
323560.fig.008a
(a)
323560.fig.008b
(b)
323560.fig.008c
(c)