High Tap Density Spherical Cathode Material Synthesized via Continuous Hydroxide Coprecipitation Method for Advanced Lithium-Ion Batteries

Table 1

Calculated structure parameters for Li [Ni0.5Mn0.3Co0.2]O2.

Samplea-axis (Å)c-axis (Å)Unit volume (Å3)c/a

Prepared Li[Ni0.5Mn0.3Co0.2]O22.87014.256101.6904.9671.779
Li[Ni0.5Mn0.3Co0.2]O2 [10]2.90814.250104.44.901.50
Li[Ni0.5Mn0.3Co0.2]O2 [11]~2.87~14.26~102~4.9631.20