Review Article

The Use of Diamond for Energy Conversion System Applications: A Review

Figure 3

Cyclic voltammograms recorded at BDD and BDD-IrO2 ( ) electrodes in 0.5 M H2SO4. Scan rate: 100 mV s−1. Geometric surface area 1 cm2. corresponds to 1015 molecules IrO2 cm−2 (reprinted with permission from [21]).
675124.fig.003