Review Article

The Use of Diamond for Energy Conversion System Applications: A Review

Figure 4

SEM images at two different magnification scales of a BDD-Pt electrode prepared by electrodeposition with a single potential step (5 s) from 1 to 0.02 V in a N2-saturated 2 mM H2PtCl6 + 1 M HClO4 solution (reprinted with permission from [21]).
675124.fig.004a
(a)
675124.fig.004b
(b)