Figure 5

Cyclic voltammograms of electrodeposited Pt particles on BDD electrode. Recorded in a N2-saturated 1 M HClO4 solution at 50 mV s−1 and 25°C. Conditions of electrodeposition: single potential step (5 s) from 1 to 0.02 V in a N2-saturated 2 mM H2PtCl6 + 1 M HClO4 solution (reprinted with permission from [21]).