Figure 20:
Concentration dependence of the lattice parameter
𝑎
of the
𝐹
𝑒
1
0
0
−
𝑥
𝐶
𝑜
𝑥
particles produced at an argon pressure of (1) 67, (2) 133, (3) 400, and (4) 1330 Pa.