Varied morphology when isothermally oxidised at 800°C–1200°C for 16 h.
251495.fig.003a
(a) 800°C
251495.fig.003b
(b) 900°C
251495.fig.003c
(c) 1000°C
251495.fig.003d
(d) 1100°C
251495.fig.003e
(e) 1200°C