Research Article

Influence of Milling Media on the Mechanical Alloyed W-0.5 wt. Ti Powder Alloy

Table 1

Crystallite size and lattice strain values of MA’d W-0.5 wt.% Ti powders in different milling media.

Milling mediaPure WEthanolIPAAr
MA time (h)102010201020

Crystallite size L (nm)510.4761.0057.0741.3017.276.534.93
Crystallite size G (nm)436.9031.1730.1320.6713.305.735.57
Lattice strain L0.00290.03570.34090.34021.48232.17843.4140
Lattice strain G0.00240.04360.63080.46361.80152.52553.5669