Oxidation/Corrosion Behaviour of ODS Ferritic/Martensitic Steels in Pb Melt at Elevated Temperature

Figure 1

Morphology and elemental amount of scales formed on Fe-9Cr ODS steel after exposure to static oxygen-saturated Pb-melt at 550°C for (a) 240 h and (b) 500 h.