Review Article
Parametric Conversion in Micrometer and Submicrometer Structured Ferroelectric Crystals by Surface Poling
| Substrate | QPM period (Λ) | Photoresist thickness | Pulse duration | Reference |
| LT | 20.8 μm | 1.7 μm | 500 μs | [45] | LN | 3.2 μm | 2.0 μm | 400 μs | [53] | LT | 2.0 μm | 1.3 μm | 300 μs | [40, 41] | LT | 1.5 μm | 1.3 μm | 300 μs | [54, 55] |
|
|