Research Article
Differences in Nanosecond Laser Ablation and Deposition of Tungsten, Boron, and WB2/B Composite due to Optical Properties
Figure 1
Target surface temperature and laser intensity during first 40 ns (). (a) Tungsten target and (b) boron target. Broken line denotes case without plasma absorption.
(a) |
(b) |