Research Article
Differences in Nanosecond Laser Ablation and Deposition of Tungsten, Boron, and WB2/B Composite due to Optical Properties
Figure 2
SEM micrograph (×1000) of deposited films: (a) boron 355 nm, (b) boron 1064 nm (c) tungsten 1064 nm, and (d) tungsten 355 nm. J/cm2.
(a) |
(b) |
(c) |
(d) |