Differences in Nanosecond Laser Ablation and Deposition of Tungsten, Boron, and WB2/B Composite due to Optical Properties

Figure 4

The cross section of crater from experiment (blue line) and theoretical calculation (yellow line). Target: tungsten; laser wavelength 355 nm; fluence 10 J/cm2; 50 laser pulses.