Differences in Nanosecond Laser Ablation and Deposition of Tungsten, Boron, and WB2/B Composite due to Optical Properties
Figure 6
SEM micrograph of deposited WB3 film (magnification ×5000) with EDS measurement points (a) and the abundances of elements in the deposited film in the spot spectrum 3 (b) and table reporting the composition of the film in examined areas (c).
(a) |
(b) |
(c) |