Research Article

Optical Study on Poly(methyl methacrylate)/Poly(vinyl acetate) Blends

Figure 1

FT-IR spectra of (a) pure PMMA, (b) a blend of (50/50 PMMA/PVAc), and (c) pure PVAc before (—) and after exposure to UV radiation (- - -) for 24 hours.
150389.fig.001a
(a)
150389.fig.001b
(b)
150389.fig.001c
(c)