Research Article

Influence of Parameters of Cold Isostatic Pressing on TiO2 Films for Flexible Dye-Sensitized Solar Cells

Figure 4

TEM images of TiO2 films (a) without CIP and (b, c) with a CIP pressure of 200 MPa and holding time of 600 s. The small inset shows the higher magnification image of each sample.
410352.fig.004a
(a)
410352.fig.004b
(b)
410352.fig.004c
(c)