Research Article

Influence of Parameters of Cold Isostatic Pressing on TiO2 Films for Flexible Dye-Sensitized Solar Cells

Figure 5

Nyquist impedance results of DSCs after various CIP processes. (a) Schematic diagram of the –Im(Z) versus Re(Z) curve; (b) Nyquist impedance results of samples without CIP and with CIP at different pressures for 300 s; (c) Nyquist impedance results of samples with the same CIP pressure of 200 MPa but different holding time; (d) calculated overall internal resistance of TiO2 films after various CIP pressing. The overall internal resistance of the sample without pressing is 55 ohm.
410352.fig.005a
(a)
410352.fig.005b
(b)
410352.fig.005c
(c)
410352.fig.005d
(d)