Research Article
Influence of Parameters of Cold Isostatic Pressing on TiO2 Films for Flexible Dye-Sensitized Solar Cells
Figure 7
TiO2 film thicknesses after CIP compressing at different conditions; the film thickness before CIP pressing was 8.2 μm.