Research Article

Enhanced Photoactivity of Fe + N Codoped Anatase-Rutile Nanowire Film under Visible Light Irradiation

Table 1

The average crystallite size of anatase TiO2 and the content of rutile, anatase for undoped, Fe-doped, nitrogen-doped, and codoped TiO2 nanowires.

Undoped TiO2Fe-doped TiO2N-doped TiO2 codoped TiO2

Content of rutile (wt%)21.8819.6622.4821.89
Content of anatase (wt%)78.1280.3477.5278.11
Average crystallite size of anatase (nm)32.9225.2727.6027.78
Average crystallite size of rutile (nm)30.5725.3026.9328.78