Research Article

Effect of Accelerated Thermal Ageing on the Selective Solar Thermal Harvesting Properties of Multiwall Carbon Nanotube/Nickel Oxide Nanocomposite Coatings

Figure 6

Fingerprint Raman spectra for a typical before and after thermal ageing test. The main phonon peaks due to NiO (~524 and ~1100 cm−1) and carbon (  cm−1 and  cm−1) clearly show a loss of carbon after ageing test.
678394.fig.006