Review Article
Zinc-Based Semiconductors/Polymer Thin Films Junction for Photovoltaic Application
Table 1
The electrolyte, composition and its conductivity at room temperature.
| Chitosan | PEO | NH4I | σ | (g) | (g) | Wt. % | (g) | (S cm−1) |
| 0.25 | 0.25 | 0 | 0.000 | () × 10−10 | 0.25 | 0.25 | 5 | 0.026 | () × 10−10 | 0.25 | 0.25 | 10 | 0.055 | () × 10−10 | 0.25 | 0.25 | 15 | 0.088 | () × 10−9 | 0.25 | 0.25 | 20 | 0.125 | () × 10−8 | 0.25 | 0.25 | 25 | 0.166 | () × 10−8 | 0.25 | 0.25 | 30 | 0.214 | () × 10−8 | 0.25 | 0.25 | 35 | 0.269 | () × 10−7 | 0.25 | 0.25 | 40 | 0.333 | () × 10−7 | 0.25 | 0.25 | 45 | 0.409 | () × 10−5* | 0.25 | 0.25 | 50 | 0.500 | () × 10−6 |
|
|
*: referring to the highest conductivity at room temperature.
|