Research Article

Ultrathin Oxide Passivation Layer by Rapid Thermal Oxidation for the Silicon Heterojunction Solar Cell Applications

Figure 6

Variation of current density as a function of voltage of silicon oxide layer with thicknesses 1, 1.4, and 3.2 nm formed by rapid thermal annealing process.