Photoetching of Immobilized --PVC Composite for Improved Photocatalytic Activity
Table 3
Microstructures of TiO2 powder, nonetched TiO2-ENR50-PVC composite, and photoetched TiO2-ENR50-PVC composite.
| Samples | BET surface | Total pore | Average pore | | area (m2 gā1) | volume (cm3 gā1) | diameter (nm) |
| TiO2 powder | 10.17 | 0.0237 | 9.348 | TiO2 composite | 5.44 | 0.0161 | 11.846 | Etched TiO2 composite | 15.24 | 0.0244 | 6.418 |
|
|