Solar Photocatalytic Degradation of Bisphenol A on Immobilized ZnO or TiO2

Figure 10

Degradation of a mixture of BPA and EE2 in UPW at 1.6 mg/cm2 ZnO. Effect of (a) 100 μg/L EE2 on 50, 100 and 200 μg/L BPA; (b) 50, 100 and 200 μg/L BPA on 100 μg/L EE2. Inset graph: plot of (3).