Research Article

Supported Zinc Oxide Photocatalyst for Decolorization and Mineralization of Orange G Dye Wastewater under UV365 Irradiation

Figure 3

Effect of (a) preparation temperature and (b) mixing speed. The conditions were initial dye concentration of 50 mg L−1, ZnO loading of 60 g m−2, light intensity of 2.1 mW cm−2, and reaction time during 120 min.
595031.fig.003a
(a)
595031.fig.003b
(b)