Evaluation of Photocatalytic Active Coatings on Sintered Glass Tubes by Methylene Blue
Figure 9
Change in concentration of MB with time. MB initial concentration: 14 mg/L, UV radiation nm–420 nm, recirculating reactor open to air, absorption at 665 nm and immobilized catalysts.