Research Article

H2O2 Treatment of Electrochemically Deposited Cu2O Thin Films for Enhancing Optical Absorption

Figure 6

PEC results of (a) the as-deposited film and (b) the film treated at room temperature for 24 hours.
738063.fig.006a
(a)
738063.fig.006b
(b)