Physical Properties of Macroporous Tungsten Oxide Thin Films and Their Impact on the Photocurrent Density
Figure 2
SEM images of (a) WO3 thin film obtained using polystyrene spheres of 0.1 μm and (b) polystyrene spheres of 0.5 μm, before and after annealing at 500°C.