The particle size, band gap, and surface area of the prepared catalysts.

SampleParticle size, nmBand gap,
eV
Surface area, m2/g

ZrO2-SiO215.3 3.04418
0.1 Pt/ZrO2-SiO214.7 2.88397
0.2 Pt/ZrO2-SiO214.0 2.73363
0.3 Pt/ZrO2-SiO213.72.61354