Research Article
Photocatalytic Decolourization of Direct Yellow 9 on Titanium and Zinc Oxides
Table 2
Pseudofirst-order rate constants and half-live times for photocatalytic degradation of DY9 (80 μmol·L−1) upon irradiation with solar simulated light (500 W/m2) at varying catalysts loading (g·L−1).
|